Table 1 Mix proportion of UHPC (weight ratio).

From: Control of Tensile Behavior of Ultra-High Performance Concrete Through Artificial Flaws and Fiber Hybridization

Compound

Binder

w/b

Filler

Fine aggregate

EA

SRA

SP

Anti-foamer

Cement

Zirconia silica fume

Proportion

1

0.25

0.2

0.3

1.1

0.075

0.01

0.023–0.026

0.0007