Skip to main content

Table 4 Drying characteristics of the \( C\overline{S} A \) and portland cement pastes.

From: Pore Structure of Calcium Sulfoaluminate Paste and Durability of Concrete in Freeze–Thaw Environment

Mixture ID

Total  % weight change

Day to equilibrium (less than 0.02 %/day)

\( C\overline{S} A \) 0.4a

−9.9

24 days

\( C\overline{S} A \) 0.5

−15.3

24 days

\( C\overline{S} A \) 0.6

−20.3

24 days

PC 0.4b

−15.9

50 days

PC 0.5

−21.7

50 days

PC 0.6

−26.0

41 days

  1. aThe mixture ID \( C\overline{S} A \) 0.40 stands for the \( C\overline{S} A \) cement pastes or concrete with a water-to-cement ratio of 0.4.
  2. bThe mixture ID PC 0.40 stands for the portland cement pastes or concrete with a water-to-cement ratio of 0.4.