Table 1 Constituents and proportions of ultra-high performance mortars (kg/m3).

From: Pull-Out Behaviour of Hooked End Steel Fibres Embedded in Ultra-high Performance Mortar with Various W/B Ratios

Type

UHPM1

UHPM2

UHPM3

Constituent

 

Kg/m3

 

Cement type III 52.5 N

710

710

710

Silica fume

231

231

231

Ground quratz

211

211

211

Fine sand

1020

1020

1020

Superplasticizer

30.7

30.7

30.7

Accelerator

30

30

30

Water

140.7

186.7

243.7

W/B

0.15

0.20

0.25