From: Evaluation of Crack Propagation and Post-cracking Hinge-type Behavior in the Flexural Response of Steel Fiber Reinforced Concrete
Specimen
Mean compressive strength (MPa)
SD (MPa)
Control
34.6
1.05
SFRC50
34.4
0.82
SFRC75
40.4
1.88