Fig. 7From: Experiments on Tensile and Shear Characteristics of Amorphous Micro Steel (AMS) Fibre-Reinforced Cementitious CompositesMeasured tensile stress and strain curves depending on the volume of steel fibre for two fibre length of L = 15 mm and 30 mm. a L = 15 mm (0.75%), b L = 15 mm (1.0%), c L = 15 mm (1.25%), d L = 15 mm (1.50%), e L = 30 mm (0.75%), f L = 30 mm (1.0%), g L = 30 mm (1.25%), h L = 30 mm (1.50%).Back to article page