Skip to main content

Table 2 Size distribution of waste glass powder (after 50 min milling).

From: Mitigation Effect of Waste Glass Powders on Alkali–Silica Reaction (ASR) Expansion in Cementitious Composite

Particle size

< 20 (μm)

20–38 (μm)

38–53 (μm)

53–75 (μm)

75–150 (μm)

150–300 (μm)

300–600 (μm)

600–900 (μm)

> 900 (μm)

Percentage (%)

11.0

18.5

27.7

22.6

9.1

8.1

1.1

0.8

1.1