From: Mitigation Effect of Waste Glass Powders on Alkali–Silica Reaction (ASR) Expansion in Cementitious Composite
Items
SiO2
Al2O3
Fe2O3
CaO
MgO
Na2O
K2O
SO3
TiO2
Cr2O3
Waste glass powder
70.40
3.37
0.508
9.20
1.00
13.78
0.663
0.38
0.053
0.094
Fly ash
58.46
28.90
3.15
2.63
1.08
0.72
1.72
1.35
–