From: Dynamic Properties of Strain-Hardening Cementitious Composite Reinforced with Basalt and Steel Fibers
Specimen ID
BF0SF0
BF3SF0
BF2.5SF0.5
BF2SF1
Compressive strength (MPa)
30.2
34.1
32.6
33.9
Tensile strength (MPa)
3.24
3.87
3.92
4.13