Fig. 5From: Experimental Study on Damage Evaluation, Pore Structure and Impact Tensile Behavior of 10-Year-Old Concrete Cores After Exposure to High TemperaturesThe frequency domains of specimens under different impact loads a 20 °C; b 600 °C.Back to article page