From: Shear Capacity Contribution of Steel Fiber Reinforced High-Strength Concrete Compared with and without Stirrup
Surface area (cm2/g)
Density (g/cm3)
Ig.loss (%)
Chemical composition (%)
SiO2
Al2O3
Fe2O3
CaO
MgO
SO3
3413
3.15
1.40
21.25
5.28
3.02
61.00
3.71
1.24