Table 2 Slump and mechanical properties.

From: Energy Absorption Characteristics of PVC Coarse Aggregate Concrete under Impact Load

Specimen code

Compressive strength (MPa)

Elastic modulus (GPa)

Splitting strength (MPa)

Slump (mm)

NC

49.34

4.06

4.16

185

CA5%

43.32

3.97

3.37

181

CA10%

39.92

3.81

2.99

179

CA15%

38.3

3.44

2.76

171

CA20%

33.8

3.26

2.39

165

CA30%

28.82

2.91

2.21

160