Fig. 7
From: Utilization of Recycled Aggregate Concrete for Marine Site Based on 7-Year Field Monitoring
![Fig. 7](http://media.springernature.com/full/springer-static/image/art%3A10.1186%2Fs40069-021-00473-w/MediaObjects/40069_2021_473_Fig7_HTML.png)
Relationship between compressive strength at 28 days and Dc of NA and RCA concretes after being exposed to seawater for 7 years.
From: Utilization of Recycled Aggregate Concrete for Marine Site Based on 7-Year Field Monitoring
Relationship between compressive strength at 28 days and Dc of NA and RCA concretes after being exposed to seawater for 7 years.