Fig. 6From: Investigating the Hybrid Effect of Micro-steel Fibres and Polypropylene Fibre-Reinforced Magnesium Phosphate Cement Mortara Compressive strength of PS8 and fPS4 at different curing ages and b, c compressive strength of MPC mortar with 1.6% hybrid fibres and 1.6% PP fibres, respectively, after curing for 7Â days.Back to article page