Fig. 3From: Performance of CO2-Cured Alkali-Activated Slag Pastes During Curing and ExposureXRD patterns of CO2-cured alkali-activated BFS (with different activator concentrations) subjected to (a) further water bath curing and (b) seawater immersionBack to article page