From: Experimental Investigation on the Effect of Curing Condition and Admixture on Meso-Structure of Recycled Aggregate Concrete Based on X-ray CT
Sample No
RACC
RACS
RACSF
RACS6012
RACS8009
Compressive strength
59.6
61.4
51.9
56.7
54.6