Table 5 Percentage value of pore surface area in different ranges (%)

From: Experimental Investigation on the Effect of Curing Condition and Admixture on Meso-Structure of Recycled Aggregate Concrete Based on X-ray CT

Range of pore surface area/mm2

0–0.1

0.1–0.2

0.2–0.4

0.4–0.6

0.6–0.8

0.8–1.0

RACC20

56.57

18.92

14.41

5.72

2.76

1.63

RACS20

63.42

17.20

11.82

4.28

2.07

1.20

RACSF20

58.78

18.26

13.53

5.27

2.56

1.60

RACS6012

52.90

20.52

15.82

6.12

2.89

1.76

RACS8009

58.78

18.26

13.53

5.27

2.56

1.60