Skip to main content

Table 10 Test results (compressive strength) with the introduction of additive No. 1 with the addition of 40.5 g

From: Research of Nano-modified Plain Cement Concrete Mixtures and Cement-Based Concrete

Day 3

Day 7

Day 28

Cube 1

Cube 1

Cube 1

2490 g–120 kg/s-37.4 MPa

2440 g–158 kg/s-49.3 MPa

2415 g–83 kg/s-26.2 MPa

Cube 2

Cube 2

Cube 2

2500 g–140 kg/s-43.5 MPa

2460 g–162 kg/s-50.4 MPa

2400 g–102 kg/s-32 MPa

40.45 MPa /39.29

49.8 MPa /39.29

29.1 MPa /39.29

102.9

126.9

74.0