Table 7 Compressive strength loss rate of five groups by dry–wet test

From: Experimental Investigation on the Properties of Sustainable Pervious Concrete with Different Aggregate Gradation

Groups

Original strength (MPa)

Strength of dry–wet test (MPa)

Loss rate (%)

20 cycles

COV (%)

30 cycles

COV (%)

40 cycles

COV (%)

20 cycles

30 cycles

40 cycles

A

15.26

15.06

1.40

14.73

1.54

14.41

1.98

1.3

3.5

5.6

B

13.47

12.72

1.91

12.15

2.46

11.52

2.18

5.6

9.8

14.5

C

11.53

10.63

2.06

10.32

3.47

9.93

2.86

7.8

10.5

13.9

D

8.13

7.15

3.39

6.67

4.51

6.38

5.44

12

17.9

21.5

E

5.97

4.70

5.05

4.36

6.08

3.59

7.73

21.3

27

39.8