Skip to main content

Table 4 Fresh properties of concrete

From: Thermal Cracking in High Volume of Fly Ash and GGBFS Concrete

Sample ID

Slump (mm)

Air content (%)

Density (kg/m3)

N50-0

75

2.5

2441

N50-FA30

30

4.8

2383

N50-G60

65

4

2445