Table 6 Results of wet packing density test with recycled sand

From: Mechanical Properties of Ultra-High Performance Concrete (UHPC) and Ultra-High Performance Fiber-Reinforced Concrete (UHPFRC) with Recycled Sand

Index

Solid ratio

Void ratio

Loose

Rodded

Vibrated

Loose

Rodded

Vibrated

W-RS-1

0.7748

0.7747

0.7866

0.2252

0.2253

0.2134

W-RS-2

0.7753

0.7767

0.7871

0.2247

0.2233

0.2129

W-RS-3

0.7868

0.7912

0.7934

0.2132

0.2088

0.2066

W-RS-4

0.7836

0.7815

0.7926

0.2164

0.2185

0.2074