Table 4 Mixing ratio of RAC beams (kg/m3)

From: Study on Crack Resistance and Calculation Model of RAC Beams Strengthened with Prestressed CFRP

Serial number

Cement

Water

Natural coarse aggregate

Natural fine aggregate

Recycled coarse aggregate

Additional water

RAC0

360

180

1209

651

0

0

RAC40

360

180

725

651

429

18.02

RAC70

360

180

363

651

750

31.50

RAC100

360

180

0

651

1071

44.98