From: Increasing the Length of Concrete Pavement Slabs Using Shrinkage Reducing Admixture and Polypropylene Fiber
Concrete type
Fc (MPa)
Ec (MPa)
Sc (MPa)
D (mm)
OPC 0.35
53.58
34,915.62
8.36
204
SRA 0.35
51.34
34,177.97
7.65
215
FIBER 0.35
63.74
38,082.41
8.6
202
SRA & FIBER 0.35
57.24
36,088.45
9.01
196