From: Experimental Study on Modification of Grouting Material for Joints of Prefabricated Buildings
Average particle size (μm)
Apparent density (g cm−3)
Specific surface area (m2/g)
Fineness modulus
Bulk density (g/L)
713.22
0.93
0.0184
2.34
398.1