From: Effects of Fine LWA and SAP as Internal Water Curing Agents
Cement | Mixing water | SP | Air | Sand | LWA | SAP | Density (kg/m3) | |
---|---|---|---|---|---|---|---|---|
Reference | 0.240 | 0.225 | 0.015 | 0.01 | 0.51 | – | – | 2,286 |
CEC 1a | 0.240 | 0.225 | 0.015 | 0.01 | 0.42 | 0.09 | – | 2,161 |
CEC 1b | 0.240 | 0.225 | 0.015 | 0.01 | 0.42 | 0.09 | – | 2,123 |
CEC 2a | 0.240 | 0.225 | 0.015 | 0.01 | 0.35 | 0.16 | – | 2,078 |
Pumice 1a | 0.240 | 0.225 | 0.015 | 0.01 | 0.44 | 0.07 | – | 2,174 |
Pumice 2a | 0.240 | 0.225 | 0.015 | 0.01 | 0.38 | 0.13 | – | 1,951 |
SAP 0.3 % | 0.240 | 0.225 | 0.015 | 0.01 | 0.507 | – | 0.003 | 2,284 |
SAP 0.6 % | 0.240 | 0.225 | 0.015 | 0.01 | 0.504 | – | 0.006 | 2,260 |