Skip to main content

Table 5 Decomposition amount of calcium hydroxide.

From: Evaluation of Pozzolanic Activity for Effective Utilization of Dredged Sea Soil

 

Plain cement paste

Metakaolin

Heat treated temperature

SH at 500 °C

SH at 730 °C

JH at 420 °C

JH at 500 °C

Weight before decomposition of CH (%)

77.425

76.162

78.534

76.715

77.444

76.845

Weight after decomposition of CH (%)

74.124

73.557

75.390

73.648

74.484

74.098

Amount of CH decomposition (%)

3.301

2.605

3.144

3.067

2.960

2.747