Material

Mix# 1(8.5 MPa)

Mix# 2 (16 MPa)

Mix# 3 (25 MPa)

Cement

200 kg/m3

300 kg/m3

400 kg/m3

Sand

853 kg/m3

810 kg/m3

773 kg/m3

Coarse aggregate

853 kg/m3

520 kg/m3

496 kg/m3

Fine aggregate

481 kg/m3

520 kg/m3

496 kg/m3

Water

100 kg/m3

132 kg/m3

163 kg/m3

Superplasticizer

As required

As required

As required

Compressive strength MPa

8.5

16

25